SEMI G15 - Standard Test Method for Differential Scanning Calorimetry of Molding Compounds -

Member Price: ₩113
Non-Member Price: ₩267,000

Volume(s): Packaging
Language: English



Type: Single Standards Download (.pdf)

Revision: SEMI G15-93 (Reapproved 0811) - Inactive

Revision

Abstract


NOTICE: This Standard or Safety Guideline has an Inactive Status because the conditions to maintain Current Status have not been met. Inactive Standards or Safety Guidelines are available from SEMI and continue to be valid for use.

 

This Document describes procedures for evaluating epoxy molding compounds by differential scanning calorimetry (DSC).

 

This test method uses SI units.

 

Referenced SEMI Standards (purchase separately)

None.

 

Revision History

SEMI G15-93 (Reapproved 0811)

SEMI G15-93 (technical revision)

SEMI G15-82 (first published)

Interested in purchasing additional SEMI Standards?

Consider SEMIViews, an online portal with access to over 1000 Standards.

Refund Policy: Due to the nature of our products, SEMI has a no refund/no exchange policy. Please make sure that you have reviewed your order prior to finalizing your purchase. All sales are final.